Guests report that after anti-sublimation, the fastness is not good, and the pulling force is also poor. I would like to ask what solution we have
After hearing the feedback, the Normante printing materials engineer immediately arranged for testing and proofing development
1. (58 yuan/high elastic water-based water-based ink transparent N-99-3C 70% + 30% PU special effect anti-sublimation primer black F7 42 yuan) +2% high elastic curing agent primer 3 times
2. (58 yuan/high elastic waterproof water-based ink transparent N-99-3C 20% + 80% PU special effect anti-sublimation primer black F7 42 yuan) +2% high elastic curing agent 3 times printing
3. (58 yuan/high elasticity waterproof water-based ink white N-99-3A + +2% high elasticity curing agent 4 times printing
4, 50 yuan PU plus light paste + 1% T999-2 curing agent printed 2 times
5. After drying naturally, dry thoroughly
Remarks: The surface is contaminated with wool and adhesion